Hastelloy C-276 (UNS N10276) Seamless Pipes & Tubes Manufacturer & Supplier

Alloy C-276 (Hastelloy C-276, UNS N10276) is considered the most versatile corrosion-resistant alloy available. With 16% molybdenum, 16% chromium, and 4% tungsten in a nickel base, it resists the formation of grain-boundary precipitates in the weld heat-affected zone, making it suitable for most chemical process applications in the as-welded condition.

UNS: N10276 | Category: Nickel-Molybdenum-Chromium Alloy | Werkstoff Nr: 2.4819 | EN Name: NiMo16Cr15W

Alloy C-276 — Also Known As

Alloy C-276 is also commonly known as Alloy C-276, Hastelloy C-276 (UNS N10276) Seamless Pipes & Tubes, N10276, UNS N10276, 2.4819, Werkstoff 2.4819, W.Nr 2.4819, NiMo16Cr15W, alloy c276, c276, c-276, hastelloy c276, hastelloy c-276.

Alloy C-276 — Applicable Standards & Specifications

Alloy C-276 is commonly supplied to ASTM B622, ASME SB622, ASTM B619, ASME SB619, ASTM B626, ASME SB626, ASTM B775, ASME SB775, ASTM B829, ASME SB829.

Size Range

Outer Diameter: 1/4" NPS to 10" NPS (6.35mm to 273.1mm OD)

Wall Thickness: SCH 5S to SCH 80S

Chemical Composition (%)

NiMoCrWFeCoCMnSiV
Remainder15.0-17.014.5-16.53.0-4.54.0-7.02.5 max0.01 max1.00 max0.08 max0.35 max

Mechanical Properties

Tensile Strength
690 MPa min
Yield Strength
283 MPa min
Elongation
40% min
Hardness
N/A

Physical Properties

Density
8.89 g/cm3
Melting Range
1325-1370 C
Thermal Conductivity
10.2 W/m-K
Electrical Resistivity
1300 nOhm-m
Specific Heat
427 J/kg-K
Coeff. of Thermal Expansion
11.2 um/m-C

Corrosion Resistance

Pitting Resistance (PREN)
>70 (highest available)
Max Service Temp (Oxidizing)
1093 C
Intergranular Corrosion
Outstanding (low C)
Stress Corrosion Cracking
Virtually immune
General Corrosion Rate
Nil in most acids
Seawater Resistance
Outstanding

Applicable Standards

Applications

Industries Served

Key Advantages

Equivalent Grades

ASTM
N10276
Trade
Hastelloy C-276
DIN
2.4819