Austenitic Stainless Steel
SS 904L
UNS: N08904 | Werkstoff: 1.4539
ASTM: N08904
Austenitic Stainless Steel
SS 317L
UNS: S31703 | Werkstoff: 1.4438
ASTM: TP317L
10 differences found
7 in chemical composition, 3 in mechanical properties. Differences highlighted in gold.
Chemical Composition (% max unless range)
| Element | SS 904L | SS 317L | Match |
|---|---|---|---|
| C | 0.020 max | 0.030 max | |
| Mn | 2.00 max | 2.00 max | |
| Si | 1.00 max | 0.75 max | |
| P | 0.045 max | 0.045 max | |
| S | 0.035 max | 0.030 max | |
| Cr | 19.0-23.0 | 18.0-20.0 | |
| Ni | 23.0-28.0 | 11.0-15.0 | |
| Mo | 4.0-5.0 | 3.0-4.0 | |
| Cu | 1.0-2.0 | - |
Mechanical Properties
| Property | SS 904L | SS 317L | Match |
|---|---|---|---|
| Tensile Strength | 490 MPa min | 515 MPa min | |
| Yield Strength | 220 MPa min | 205 MPa min | |
| Elongation | 35% min | 35% min | |
| Hardness | 90 HRB max | 95 HRB max |
International Standard Equivalents
| Standard | SS 904L | SS 317L |
|---|---|---|
| UNS Number | N08904 | S31703 |
| Werkstoff Nr. | 1.4539 | 1.4438 |
| EN Name | X1NiCrMoCu25-20-5 | X2CrNiMo18-15-4 |
| ASTM / ASME | N08904 | TP317L |
| JIS (Japan) | SUS 890L | SUS 317L |
| BS (British) | - | 317S12 |
| Applicable Standards | ASTM A312 / ASME SA312, ASTM B673 / ASME SB673, ASTM B674 / ASME SB674, DIN EN 10216-5 | ASTM A312 / ASME SA312, ASTM A213 / ASME SA213, ASTM A269, DIN EN 10216-5 |